Hi:

Paul Herman gave you some excellent advice on this. Sell the cone 6 stuff
and buy some hi fire porcelain. You'll be a lot happier with the
results. You'll do a lot less work too.

The last thing you would want to do is add goldart, or any other stoneware
clay to any kind of white claybody. It wouldn't be anywhere near a
porcelain if you did that.

regards, Craig Martell Hopewell, Oregon