Sandy Henderson on sat 6 sep 03


I find that it's a lot easier to get glaze through an 80 mesh screen if I put it through a
40 or 60 mesh first. Also, with apologies to Ron Roy, I put glazes through coarser
screens (40 mesh or --I admit -- even coarser) for years without problems. Would
this make a glaze less stable? or create some other problem not easily observed?

Sandy Henderson