a spar 36.
silica 25
epk 17
whiting 14

for color and texture

talc 2.7
iron 1.6
tin 1.3
bone ash 1.0

a cone six semi gloss glaze
little fludity
stains show
warm tan in color

Ron Roy on sat 20 sep 03


Hal - are you sure everything is here? - there is no way this is going to
melt properly at cone 6.

RR