search  current discussion  categories  kilns & firing - shelves & furniture 

dannon's paper saggars

updated sun 21 sep 03

 

Lori Leary on sat 20 sep 03


Dannon,
If you are on list could you drop me a line, I have lost your email =
address...

Anyone else:=20
Does anyone remember when Dannon's article on paper saggars appeared and =
which mag it was in? I have about a bazillion years of CM, PMI, =
Claytimes, Ceramics A&P...(all hopelessly disorganized at the moment). =
I am trying to find the article to turn someone on to using paper =
saggars.

Thanks,
Lori L.

Marta Matray Gloviczki on sat 20 sep 03


Lori Leary wrote:

>Does anyone remember when Dannon's article on paper saggars appeared and
which mag it was in?>>>


dear lori,
PMI winter 2000.
firing with paper saggar by dannon rhudy.
page 14,15 and 16
(it was easy to look it up, the issue is always on my desk!)
marta

=====
marta matray gloviczki
rochester,mn

http://www.angelfire.com/mn2/marta/
http://users.skynet.be/russel.fouts/Marta.htm
http://www.silverhawk.com/crafts/gloviczki/welcome.html