search  current discussion  categories  glazes - misc 

tony h's 20 20 glaze

updated thu 2 oct 03

 

JAMES MCCALL on wed 1 oct 03


When I fired his clear glaze to cone 7 I got bubbles not pinholes on the
outside of a vase. It was worse on the inside. I used the same base glaze
with cobalt, rutile, and tin and everything fire ok on another piece.

What went wrong with the clear base?