Jerry Dean on sat 4 oct 03
Im giving up on Majolica on my large bowls....it works great on my flat
surfaces pieces, but my large bowls are full of pinholes etc...( no need for
another discussion on this. Im tired of experimenting ) Anyway........I have
a years worth of large Thrown Red earthenware bowls in my studio, just dying
to be decorated. I can't remember a thing about where to start with low-fire
glazing. I need a workshop where we explore all low-fire glazing/decorating
techniques. I'm up for anywhere a plane can take me. Thanks Guys...Jerry
Valice Raffi on sat 4 oct 03
Jerry,
I give workshops on low-fire glazing techniques. I don't have one
scheduled at the moment, but plan on giving one in the Sacramento area
soon. You're giving me incentive to set a date!
Valice
in Sacramento
> I need a workshop where we explore all low-fire glazing/decorating
>techniques. I'm up for anywhere a plane can take me. Thanks Guys...Jerry
Jerry Dean on sun 5 oct 03
Valice.......Just let me know what time you might be thinking of.......and
you can put the word on on Clayart.Im interested in airbrush techniques, under
and over glazes and exploring what the Commercial glazes have to offer .
Thanks Jerry
| |
|