Gloria Gutridge on sat 25 oct 03
Does anyone still have a copy of the May / June 97 issue of
Claytimes. There is a recipe in there called vanilla ice cream that
I would like to try that I'm told appears in that issue. I'm also
looking for one called French Vanilla but can't seem to find it. The
artist told me she would email it to me, but she must be really busy
as it's been a couple of months now..
If someone has it and could send me the recipe I would be really
grateful....
THANKS
Gloria
Britt Britt on sat 25 oct 03
Gloria,
Here is the recipe I have.
VANILLA ICE CREAM
Custer Feldspar 49.48
EPK Kaolin 24.74
Dolomite 21.64
Gerstley Borate 2.06
Whiting 2.06
Tin Oxide 4.00
Hope that helps,
JOhn
Gloria Gutridge on sun 26 oct 03
John
Thank you very much. I have a couple of pieces that I want to try it
on..
Gloria
--- In clayart@yahoogroups.com, Britt Britt wrote:
> Gloria,
>
>
> Here is the recipe I have.
>
>
> VANILLA ICE CREAM
>
>
> Custer Feldspar 49.48
> EPK Kaolin 24.74
> Dolomite 21.64
> Gerstley Borate 2.06
> Whiting 2.06
> Tin Oxide 4.00
>
> Hope that helps,
>
> JOhn
>
>
______________________________________________________________________
________
> Send postings to clayart@l...
>
> You may look at the archives for the list or change your
subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@p...
| |
|