Heidi Haugen on mon 27 oct 03


first, i apologize for my last message making it to the list instead of
the person to whom it was addressed....my bad.

was just glazing and thinking about the rr black question and realized
there is one more thing. i do not add the 2 percent bentonite and don't
seem to have any suspension issues. that could possibly be contributing
to crawling/cracking issues.

thanks.
heidi haugen