Sandra Talarico on thu 30 oct 03
I also had many bloating problems with S266. The bloating started showing
up in larger pieces - anything over 2-3 pounds of clay. I was firing
it to cone 6 also. Cone packs all over the kiln, so I know it was 6.
I quit using it - even though I loved the way it took some of the glazes
I have.
| |
|