gordon jones on thu 30 oct 03


mel, the beat up kiln i spoke to you about converting, now think maybe
completly gut this thing put fiber between rings for gasket, itc coat and
try firing some cone 6 reduction. mark ward says the raku burner i have
would do the trick with enough pressure. has anyone tried this,7 cubic ft.i
have a 100 pound tank i can hook up was thinking maybe a 40lb for a first
try. i would only have the price of the itc involved other than the butt
ugly kiln. anyone need a few new elements for skutt 1027? contact me off
list and and i might make you very happy.
its late just shut down a 24 hour bisc firing hope to get rewarded.

gordon earthbound arts

_________________________________________________________________
Surf and talk on the phone at the same time with broadband Internet access.
Get high-speed for as low as $29.95/month (depending on the local service
providers in your area). https://broadband.msn.com