search  current discussion  categories  glazes - specific colors 

iron red -- thick or thin?

updated fri 31 oct 03

 

terryh on thu 30 oct 03


i like Ohata kaki in neutral/oxidation firing. no "reduction"
at all, to get kaki red. as a matter of fact, i've been firing
using electric kiln to 2250F, and hold for a few hours.
thin or thick, yes, less black dots in thinner application.
terry

Paul B from KY wrote
>Has anyone noticed a difference in the results of iron red
>glazes (cone 10reduction) between a thick application and
>a thin one?

terry hagiwara
terryh@pdq.net