Bonnie Staffel on wed 19 nov 03
Hi, It is my opinion that it is the frit that is settling to the bottom. I
use a material called Flocs and I believe from Axner. Keeps things afloat
or stirrable after resting. Another culprit for settling is the feldspars.
It only takes a few drops into your glaze to correct it. Hope this works
for you.
Regards, Bonnie Staffel