search  current discussion  categories  glazes - crystalline 

attention crystalline glaze potters

updated sat 29 nov 03

 

Wilton Pottery on tue 25 nov 03


ATTENTION CRYSTALLINE GLAZE POTTERS:

I have been asked by A & C Black, Publishers of my book Crystalline =
Glazes to do a second edition. This book will have a new cover, new =
photographs in full colour, and I will update with new information. In =
order to get the book out by the fall of 2004, I need to send the =
publishers my information by the end of January. I realize this is not =
much time, but I am requesting crystalline glaze potters to please send =
me either slides of your work or photos on a CD that I may use in my =
book. I need top quality photos of only one pot at a time on a plain =
background with no shadows. Please list height, glaze colorant used and =
the photo credit. I am also looking for interesting glaze recipes and =
unusual results or comments. I would also like your name, address and =
e-mail address. You may get in touch with me at wppotter@kos.net or =
write to Diane Creber, 239 Simmons Road, RR 2, Odessa, Ontario K0H 2H0 =
CANADA.
=20

Ababi on wed 26 nov 03


Hello Diane Creber.
I am glad I have the chance to thank you for your book.
It was pleasant to - none English speaking person to read your book
relatively easy.
Please enter to my site to the two crystal pages.
If you like any of the images I shall add the details.


Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il

http://ababi.active.co.il

http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm




-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Wilton
Pottery
Sent: Wednesday, November 26, 2003 6:28 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: ATTENTION CRYSTALLINE GLAZE POTTERS

ATTENTION CRYSTALLINE GLAZE POTTERS:

I have been asked by A & C Black, Publishers of my book Crystalline
Glazes to do a second edition. This book will have a new cover, new
photographs in full colour, and I will update with new information. In
order to get the book out by the fall of 2004, I need to send the
publishers my information by the end of January. I realize this is not
much time, but I am requesting crystalline glaze potters to please send
me either slides of your work or photos on a CD that I may use in my
book. I need top quality photos of only one pot at a time on a plain
background with no shadows. Please list height, glaze colorant used and
the photo credit. I am also looking for interesting glaze recipes and
unusual results or comments. I would also like your name, address and
e-mail address. You may get in touch with me at wppotter@kos.net or
write to Diane Creber, 239 Simmons Road, RR 2, Odessa, Ontario K0H 2H0
CANADA.


.

=?iso-8859-1?q?Marilu=20Tejero?= on wed 26 nov 03


I would suggest you to contact TED SECOMBE from Victoria Australia. He has taken crystaline glazes to the limits and created the most beautiful pots.

http://www.arts-exclusive.com/html/secombe.htm

the oly e-mail I can find is of his guest house.

enquiries@valleyguesthouse.com.au






www.geocities.com/SoHo/Exhibit/3051






---------------------------------
Do You Yahoo!?
Todo lo que quieres saber de Estados Unidos, América Latina y el resto del Mundo.
Visíta Yahoo! Noticias.

Tony Hansen on fri 28 nov 03


We are close to releasing Fara Shimbos Crystal Glazes II
book at digitalfire. It will also be available in print,
on CD and as a download. This is a really incredible book.
Fara has a number of her own websites on the subject and
makes herself available and gives great support to
readers of her book online. One of her sites is
www.crystalline-ceramics.info

-------8<--------
I would suggest you to contact TED SECOMBE from Victoria Australia. He=
has taken crystaline glazes to the limits and created the most beautifu=
l pots.

http://www.arts-exclusive.com/html/secombe.htm

the oly e-mail I can find is of his guest house.

enquiries@valleyguesthouse.com.au






www.geocities.com/SoHo/Exhibit/3051






---------------------------------
Do You Yahoo!?
Todo lo que quieres saber de Estados Unidos, Am=E9rica Latina y el resto =
del Mundo.
Vis=EDta Yahoo! Noticias.

_________________________________________________________________________=
_____
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclin=
k.com.

-------
Tony Hansen, http://digitalfire.com
Personal Contact Page: http://digitalfire.com/services/contact.php
Calculation/Database Software for Ceramic Industry