search  current discussion  categories  glazes - specific colors 

tony/cure the blues

updated thu 27 nov 03

 

mel jacobson on wed 26 nov 03


well, i have the cure.

open a kiln like i did today.
80 pots.
no seconds. racers all.
one crack.

fired down for three hours.
iron red to die for.
rhodes just at cone 11...a bit runny.
just the way i like it.
makes me dance.
smile.
hug the dog.
all four cone packs the same. cone 11 half way down.
top, bottom, front, back.
reduction the same on every pot.

thanks to those that are still teaching me to fire.
new glazes, new idea...and, almost 69.
this holiday show will be 5 kiln loads.
never had so many pots in one place in my life.
things are good.
i am very thankful.
mel/ things here are pink and gold/not a bit of blue.