Lee Love on thu 27 nov 03
Blues is my favorite music. Natural indigo blue is my favorite color.
I like getting blue in unusual ways, without cobalt.
I put up a photo of a blue glaze I'll test in my next firing. It is a
MacKenzie blue-gray chawan. The example in this photo is more gray that
blue (I saw it bluer at the Tokyo show.) :
http://www.livejournal.com/users/togeika/2003/11/27/
Simple recipe:
feldspar 5
whiting 3
epk 3
--
Lee In Mashiko, Japan
http://Mashiko.org