Llewellyn Kouba on fri 28 nov 03


Is it possible to do very detailed in-glaze printing on surface of
porcelain thrown ware or does one have to work with bone china? If so does
anyone know a good book reference on how to work with in-glaze screen
printing on ceramic ware? Thanks

Llewellyn Kouba
Abbey Pottery

Aebersold, Jane F on sat 29 nov 03


Llewellyn,
Good sources for printing on clay are Ceramics and Print by Paul Scott, A&C
Black Publishers, London and University of Pennysylvania Press,
Philadelphia, or the online site
http://www.printandclay.net/
for the International Museum of Print and Clay
Regards,
Jane
Norman, OK



Date: Fri, 28 Nov 2003 08:15:34 -0700
From: Llewellyn Kouba
Subject: Re: Question on Screen Printing on Porcelain

Is it possible to do very detailed in-glaze printing on surface of porcelain
thrown ware or does one have to work with bone china? If so does anyone
know a good book reference on how to work with in-glaze screen printing on
ceramic ware? Thanks

Llewellyn Kouba
Abbey Pottery