search  current discussion  categories  materials - frits 

frit 3134 and 3124

updated wed 3 dec 03

 

=?iso-8859-1?q?Marilu=20Tejero?= on sun 30 nov 03


Will somene help with the ingredients of these frits?

Thanks.


www.geocities.com/SoHo/Exhibit/3051/








---------------------------------
Do You Yahoo!?
Todo lo que quieres saber de Estados Unidos, América Latina y el resto del Mundo.
Visíta Yahoo! Noticias.

Vince Pitelka on sun 30 nov 03


> Will somene help with the ingredients of these frits?

Marilu -
Did you do a websearch for Ferro Frit? There is general information and
analysis at http://www.lagunaclay.com/volumev/fritdata.pdf, or if you want
more detailed analysis go to the Matrix website at
http://www.matrix2000.co.nz/MaterialsWeb/Materials_F.htm#Ferro%20Frit%203227

Be sure to paste the whole website address into your browser.
Good luck -
- Vince

Vince Pitelka
Appalachian Center for Craft
Tennessee Technological University
1560 Craft Center Drive, Smithville TN 37166
Home - vpitelka@dtccom.net
615/597-5376
Office - wpitelka@tntech.edu
615/597-6801 x111, FAX 615/597-6803
http://iweb.tntech.edu/wpitelka/
http://www.tntech.edu/craftcenter/

=?iso-8859-1?q?Marilu=20Tejero?= on tue 2 dec 03


Thanks Vincent, I've got a severe flu and my head is affected.
Thanks for the sites.. I'll save them for the future..




www.geocities.com/SoHo/Exhibit/3051/








---------------------------------
Do You Yahoo!?
Todo lo que quieres saber de Estados Unidos, América Latina y el resto del Mundo.
Visíta Yahoo! Noticias.

Tony Hansen on tue 2 dec 03


For really detailed info try here:
http://142.179.175.169/cermat/ceramicmaterials/material.php?id=351
and
http://142.179.175.169/cermat/ceramicmaterials/material.php?id=350

-------8<--------
> Will somene help with the ingredients of these frits?

Marilu -
Did you do a websearch for Ferro Frit? There is general information and
analysis at http://www.lagunaclay.com/volumev/fritdata.pdf, or if you want
more detailed analysis go to the Matrix website at
http://www.matrix2000.co.nz/MaterialsWeb/Materials_F.htm#Ferro%20Frit%203227

Be sure to paste the whole website address into your browser.
Good luck -
- Vince

Vince Pitelka
Appalachian Center for Craft
Tennessee Technological University
1560 Craft Center Drive, Smithville TN 37166
Home - vpitelka@dtccom.net
615/597-5376
Office - wpitelka@tntech.edu
615/597-6801 x111, FAX 615/597-6803
http://iweb.tntech.edu/wpitelka/
http://www.tntech.edu/craftcenter/

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.

-------

===============