June,=20

if you have some black iron oxide you may use the following,
according to GlazeChem, for QIT-Ilmenite:




Magnesium carbonate 9.047
Whiting 3.904
Kaolin - theoretical 18.014
Silica 2.807
Rutile 30.311
Black iron oxide 40.672
Total 100