search  current discussion  categories  materials - plaster 

plaster wedging table

updated mon 1 dec 03

 

mlkrakowski@citlink.net on sun 30 nov 03


As was suggested; if your table has a solid bottom you might drill some
holes in. DO use a hand brace and bit, because, unless you have really
good control of the drill, it is too easy to get into the plaster and
possibly chip out a chunk.

Then, for future reference: when you build the box that holds the
plaster slab, put it together with lag bolts. These will permit you to
take the sides of the box off easily when necessary--as now. In fact
if you can dismantle the "box"part of the table now, it might be an
idea to do so....