I don't have the ingredients but this is the analysis from Standards
Ceramics catalog:

Ferro Frit 3134: Na2O 10.33, CaO 20.1, B2O3 23.1, SiO2 46.5

Ferro Frit 3124: K2O 0.7, Na2O 6.3, CaO 14.1, Al2O3 9.9, B2O3 13.7, SiO255.3