Maid O'Mud on wed 3 dec 03
I bought a kiln from Tucker mid September. It is a Shimpo with extra =
insulation, bottom element, rated ^10 with 3 zone Bartlett controller.
After the 6th glaze firing, I was banging my head into the wall, =
wondering why I waited so damn long to get a _good_ kiln. No more =
pinholes, no more running, no playing with switches and peering peering =
peering into peepholes. I DO use cones to confirm the computer; =
probably a habit I will always have.
Just my 2 cents.
Sam - Maid O'Mud Pottery
Melbourne, Ontario CANADA
=20
"First, the clay told me what to do.
Then, I told the clay what to do.
Now, we co-operate."
sam 1994
=20
http://www.ody.ca/~scuttell/
| |
|