Ababi on sat 6 dec 03
Please visit this page
http://members4.clubphoto.com/ababi306910/1310421/
Scroll down to my latest tests. Even when you cannot duplicate this
glaze you can see the behavior of the glaze when I increase/decrease the
different materials.
Note my simple crystal glaze in a crystal firing ^6 of course.
I shall repeat it in a regular ^6 fire.
This glaze stretches the limits of ^6 crystal glazes. This is its main
importance.
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://members4.clubphoto.com/ababi306910/
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm
| |
|