Fredrick Paget on thu 11 dec 03
>Anybody out there have a link or other reference where I could find the
>temperature/millivolt equivalence chart for the Axner OxyProbe? I seem to
>have misplaced my instruction book, so I don't know what the temperature
>readings mean. I have the reduction vs. temperature plot. I just need the
>temperature vs. meter reading plot.
>Bruce "it's around here somewhere" Girrell
That should be available on the web since it is a platinum
thermocouple. Seems to me that someone posted a reference to where
these charts were on the web a few months ago. You have to find out
which kind of platinum thermocouple it is though - Type S or Type R?
Possibly Omega has the chart on their web site. I know it is in the
set of books that they put out because I have a copy somewhere....
Fred
--
From Fred Paget, Marin County, California, USA
fredrick@well.com
Bruce Girrell on thu 11 dec 03
Anybody out there have a link or other reference where I could find the
temperature/millivolt equivalence chart for the Axner OxyProbe? I seem to
have misplaced my instruction book, so I don't know what the temperature
readings mean. I have the reduction vs. temperature plot. I just need the
temperature vs. meter reading plot.
Thanks
Bruce "it's around here somewhere" Girrell
Our house is connected to a large vortex or black hole related to all those
other mysterious singularities associated with sock-eating washing machines.
Ours causes scissors, exposed film, and instruction manuals to vanish (along
with many other items that have been lost long enough that I can't remember
them now).
Leonard Smith on fri 12 dec 03
Dear Bruce
if you do not get a link, contact me off line I have excel spreadsheets
for Type R (the one for the oxyprobe) Type K and Type N (nicrosil)
On Friday, December 12, 2003, at 06:51 AM, Bruce Girrell wrote:
> Anybody out there have a link or other reference where I could find the
> temperature/millivolt equivalence chart for the Axner OxyProbe? I seem
> to
> have misplaced my instruction book, so I don't know what the
> temperature
> readings mean. I have the reduction vs. temperature plot. I just need
> the
> temperature vs. meter reading plot.
>
Leonard Smith
Rosedale Street Gallery
2A Rosedale Street
Dulwich Hill NSW 2203
Australia
John Anthony on fri 12 dec 03
HI Bruce- I have the Axner manual handy which has the type R chart in
it.
Email me if you'd like me to fax it to you-
John Anthony
http://www.redhillpottery.com
John K Dellow on sat 13 dec 03
I don't know if the Axner one is the one made in Australia but the
Aussie one is
http://www.cof.com.au/aos.htm
John
Leonard Smith wrote:
> Dear Bruce
>
> if you do not get a link, contact me off line I have excel spreadsheets
> for Type R (the one for the oxyprobe) Type K and Type N (nicrosil)
>
>
> On Friday, December 12, 2003, at 06:51 AM, Bruce Girrell wrote:
>
>> Anybody out there have a link or other reference where I could find the
>> temperature/millivolt equivalence chart for the Axner OxyProbe? I seem
>> to
>> have misplaced my instruction book, so I don't know what the
>> temperature
>> readings mean. I have the reduction vs. temperature plot. I just need
>> the
>> temperature vs. meter reading plot.
>>
> Leonard Smith
> Rosedale Street Gallery
> 2A Rosedale Street
> Dulwich Hill NSW 2203
> Australia
>
> ______________________________________________________________________________
>
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
--
John Dellow "the flower pot man"
From the land down under
Home Page http://www.welcome.to/jkdellow
http://digitalfire.com/education/people/dellow/
| |
|