This is for you glaze experts and any lurkers who also work with glass.
Anyone know if it possible to find out the COE rating of a cone 06 gloss glaze and also of a cone 5 gloss glaze? And if so where and how?

I am trying to figure out if there is someway I can adjust a glaze so it would have more compatibility when fusing to glass with a COE 90 or 96.

Barbara Kobler http://www.claywoman.net

Ron Roy on thu 18 dec 03


Hi Barbara,

In chapter 5 in our book - page 81 you will find a high expansion glaze -
it will be the one closest to your glass.

Do a line blend between that one and the one on page 79.

If it takes a higher expansion glaze to work I can design one for you.

RR



>This is for you glaze experts and any lurkers who also work with glass.
>Anyone know if it possible to find out the COE rating of a cone 06 gloss
>glaze and also of a cone 5 gloss glaze? And if so where and how?
>
>I am trying to figure out if there is someway I can adjust a glaze so it
>would have more compatibility when fusing to glass with a COE 90 or 96.
>
>Barbara Kobler http://www.claywoman.net


Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0
Phone: 613-475-9544
Fax: 613-475-3513