John Rodgers on sun 14 dec 03
Can anyone point me to information, web sites, or where-ever for info on
crystal glazes that mature at cone 8 or less???
Anything would help.
Thanks,
John Rodgers
Chelsea, AL
Ababi on mon 15 dec 03
Yes
Mine as well as
Fara's
http://crystalline-ceramics.info/
http://crystalline-ceramics.info/bbs/index.cgi
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm
-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of John
Rodgers
Sent: Sunday, December 14, 2003 11:23 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Crystal Glazes at less than Cone 10
Can anyone point me to information, web sites, or where-ever for info on
crystal glazes that mature at cone 8 or less???
Anything would help.
Thanks,
John Rodgers
Chelsea, AL
________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org
You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/
Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
Fara Shimbo on mon 15 dec 03
I have a few of these on my website:
http://crystalline-ceramics.info
There is also a BBS on this site at
http://crystalline-ceramics.info/bbs/index.cgi
and several of the contributors fire either often
or exclusively at ^5 and ^6. They'd be thrilled
to yack to you about it all day long.
Hang in there,
Fa
--
===========================================================
Fara Shimbo, Master Crystalliere, Certified Public Nuisance
-----------------------------------------------------------
Shimbo Pottery, P.O. Box 41, Hygiene, Colorado 80533 USA
720.272.0442 7AM to 2 PM, Mountain Time
www.crystalline-ceramics.info www.shimbopottery.com
Silly Science Fiction: http://klysadel.net
===========================================================
william schran on tue 16 dec 03
John - Sure, I've been doing crystalline glazes at cone 6 for a few
years and gotten good results. Wrote an article for ClayTimes on this
subject in the Sept/Oct. 2000 issue. Listed a couple of most
successful recipes and discussed firing schedule. If you can't get a
hold of a copy, send me an email directly and I'll copy the info and
send it via postal mail.
Fara Shimbo has an e-book out on crystalline glazes and I found some
of her glazes listed for a higher cone worked just fine at cone 6.
Here's her web site: http://crystalline-ceramics.info/
Bill
>Can anyone point me to information, web sites, or where-ever for info on
>crystal glazes that mature at cone 8 or less???
>
>Anything would help.
>
>Thanks,
>
>John Rodgers
>Chelsea, AL
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.
| |
|