search  current discussion  categories  glazes - misc 

i forgot one glaze test, c2515 and its pic

updated wed 17 dec 03

 

Theresa Sandin on tue 16 dec 03


C2515, Cone 6 ox

Soda spar 50
Dolomite 25
China Clay 15
Bone Ash 10

On white vingerling clay with slip decoration with additions of 10% rio,
2% cobalt ox, 2% copper oxide.

It's super smooth, I love the way it runs and the "tooth yellow" that
turns pink in some places. Like all my glazes except my liner, it crazes.

http://www.kahlin.net/noir/keramik/c.jpg

Theresa