Theresa Sandin on fri 19 dec 03
Hi Alisa!
I live in Stockholm! I used to live in Laurel, MS for a while, but now I'm
back in my own country.
I have tested the floating green with soda feldspar instead of "nephsy"
and then it turned out more teal green, but still variegated to some
extent. I'm scanning it as I write. Could be that I somehow missed the
amounts of titania in the first test, so that it is more than 2%.
I sent you a personal email some time ago, to the e-mail you state on your
homepage. Have you recieved it?
Theresa
| |
|