Bill Edwards on thu 18 dec 03
Metastannic Acid
used in ceramic colors, colorants, glazes, stains
Metastannic acid is combined with other oxides to make
the color of maroon (or tin-red), also has the
opacifying function.
Product Name
Metastannic acid
Formula H2SnO3
Atomic Weight 168.71
Date: Thu, 18 Dec 2003 11:10:22 +1030
From: iandol
Subject: Chromium and other contaminates
Dear Bill Edwards,
Thank you for that well argued essay on Chrome and
other delights.
So, what is the pink colour. Is it Stannous Chromate?
Best regards,
Ivor Lewis. Redhill, South Australia
=====
http://www.geocities.com/tallapoosarivergallery/index.html (Coming soon)
http://www.tallapoosariverpottery.com/
"Anyone whose panties get in a bunch over what I have to say from my
tiny corner oughta order some bigger roomier panties....!" A candle for Arti
Bill Edwards
PO Box 367
Camp Hill, Alabama. 36850
__________________________________
Do you Yahoo!?
New Yahoo! Photos - easier uploading and sharing.
http://photos.yahoo.com/
| |
|