search  current discussion  categories  glazes - specific colors 

rr black revisited

updated sun 21 dec 03

 

redhat@digisys.net on sat 20 dec 03


we had a discussion within the last couple of months about rr black issues=

so i don't want to repeat myself too much but this is truly the best glaze=

for me hands down as far as fit/consistency/durability=2E=2E=2Ei adore it=2E=
=20

i use the 2 percent cobalt version, dip for 10 count on cone 04 bisque=2E=
=20
used to have a few crawling issues around the rims when i glazed by fillin=
g
the inside of the bowl then dipped the top of the outside=2E=2E=2Ewas gett=
ing a
double coat around the rim and if rr black is too thick it will crawl=2E =
i
don't believe it's a dust issue, i think it's glaze thickness that creates=

the crawling=2E i also do not add the bentonite, haven't needed it=2E

just my experience=2E