Guy Watson on sun 28 dec 03


I am trying to make a clear base glaze from raw materials (no frits) for
cone 05 My test glazes are milky (micro bubbles) Does anyone have a
reliable, tested, clear glaze I could try. I am using terracotta that
bisques at 980c and glaze fires at 1030c. Thanks for the help.---Guy