search  current discussion  categories  materials - misc 

uranium in fiesta war

updated wed 14 jan 04

 

terryh on sat 10 jan 04


>Date: Thu, 8 Jan 2004 19:30:17 -0800
>From: Zoe Johnson
>Subject: Re: Uranium in Fiesta Ware
>
>I have been told by health physicists from Los Alamos and Sandia National
>Labs who are incredibly cautious by nature that unless you are sleeping
>with the fiestaware, the danger is negligible.

the health problem of uranium in glaze is not of radiation.
i think it is from leaching out of heavy metal uranium in acidic foods.

terry hagiwara
terryh@pdq.net
http://www.geocities.com/terry.hagiwara

John Baymore on mon 12 jan 04



>I have been told by health physicists from Los Alamos and Sandia Nationa=
l
>Labs who are incredibly cautious by nature that unless you are sleeping
>with the fiestaware, the danger is negligible.

the health problem of uranium in glaze is not of radiation.
i think it is from leaching out of heavy metal uranium in acidic foods.



Was the Fiesta War just before World War I or after it?

Maybe try looking in the CLAYART archives on this topic.... there was a L=
OT
of discussion about it in the past. As I remember, the Fiestaware contai=
ns
not only uranium but thorium....which was a contaminant of the impure
uranium compounds used as colorants. Monona Rossol documented the
situation with some results from a testing program that was done on the
wares at one point if I am remembering correctly. I also think that
information was published in Clay Times at one point.


best,

..........................john


John Baymore
River Bend Pottery
22 Riverbend Way
Wilton, NH 03086-5812 USA

JBaymore@compuserve.com
http://www.JohnBaymore.com

603-654-2752 (studio)
800-900-1110 (studio)

Joe Coniglio on tue 13 jan 04


I heard a story a while back of a guy who collected noting but yellow
uranium fiesta ware. A massive amount of it. It revealed itself by
giving up a satelite signature from space and it was confiscated.

One part for sure. For some reason it really was confiscated.

wayneinkeywest on tue 13 jan 04


Darn! When I first read that, I thought
you wrote Thorazine...and was all set to
go hit Ebay and my local antique shop :>)
Wayne Seidl

As I remember, the Fiestaware contains
not only uranium but thorium....which was a contaminant of the impure
uranium compounds used as colorants.