Linda Pahl on sat 17 jan 04
Does anyone know the analysis of Fusion Frit F-38? Was not listed on
either the Insight or Matrix materials database.
Thanks in advance for any assistance.
Regards,
Linda Pahl, Kew Gardens, New York
TheClosetPotter@earthlink.net
(I throw on my wheel in my hall closet; the only possible solution in
this tiny apartment!)
Linda Pahl on sat 17 jan 04
Well, I answered my own question. I thought I was stumped as I
couldn't find the analysis anywhere but I kept at it and finally found
the page that gave the analysis for *all* of Fusions Frits:
http://www.fusionceramics.com/fritspec.htm
Linda Pahl, Kew Gardens, New York
TheClosetPotter@earthlink.net
(I throw on my wheel in my hall closet; the only possible solution in
this tiny apartment!)
Ababi on sat 17 jan 04
Hello Linda
http://www.fusionceramics.com/
Go to Frit Specification
Keep on testing (fearless...)
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm
-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Linda Pahl
Sent: Saturday, January 17, 2004 10:12 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Analysis of Fusion Frit F-38
Does anyone know the analysis of Fusion Frit F-38? Was not listed on
either the Insight or Matrix materials database.
Thanks in advance for any assistance.
Regards,
Linda Pahl, Kew Gardens, New York
TheClosetPotter@earthlink.net
(I throw on my wheel in my hall closet; the only possible solution in
this tiny apartment!)
________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org
You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/
Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
Logan Oplinger on sun 18 jan 04
On Sat, 17 Jan 2004 05:23:05 -0500, Linda Pahl
wrote:
>Well, I answered my own question. I thought I was stumped as I
>couldn't find the analysis anywhere but I kept at it and finally found
>the page that gave the analysis for *all* of Fusions Frits:
>
>http://www.fusionceramics.com/fritspec.htm
>
>Linda Pahl, Kew Gardens, New York
>TheClosetPotter@earthlink.net
Hello Linda,
Just to be sure you are aware, the Fusion Frits table from the link you
provided gives the analyses in PERCENTAGES, not oxide equivalents based on
the unity formula for fluxing oxides. For equivalents you can link to:
http://digitalfire.com/material/index.htm
or for F-38:
http://digitalfire.com/material/m-01b1x0.htm
Logan Oplinger
Another Tropical Island
Lawrence Ewing on sun 18 jan 04
Hi Linda,
Matrix V5 has a database specially for Fusion Frits. You will find F-38
included in that list.
Cheers,
Lawrence Ewing
21 Slant St
Careys Bay
Dunedin
New Zealand
EMAIL: lewing@clear.net.nz
URLS:
Matrix Glaze Software:
http://www.Matrix2000.co.nz
Glaze Chemistry Instruction:
http://www.Matrix2000.co.nz/GlazeTeach/Index.htm
New Zealand Society of Potters website:
http://www.nzPotters.com
----- Original Message -----
From: "Linda Pahl"
To:
Sent: Saturday, January 17, 2004 9:11 PM
Subject: Analysis of Fusion Frit F-38
> Does anyone know the analysis of Fusion Frit F-38? Was not listed on
> either the Insight or Matrix materials database.
>
> Thanks in advance for any assistance.
>
> Regards,
>
> Linda Pahl, Kew Gardens, New York
> TheClosetPotter@earthlink.net
> (I throw on my wheel in my hall closet; the only possible solution in
> this tiny apartment!)
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
| |
|