low fired flame ware

updated wed 21 jan 04

 

Mary Johnson on mon 19 jan 04


I have looked many resources about flame ware, and mostly are about high
fired body. Does any one know any thing about very low fired ware (in the
result of pit or bon fire) and its USUAGE on direct flame?
Thanks.

Ababi on tue 20 jan 04


In Steven Branfman revised raku book there is an explanation about this
technique,
Of course low fire!
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il