Patricia Gilmartin on tue 20 jan 04


Any suggestions for joining earthenware sculpture to marble bases? Would
E-6000 be a good choice for this too? PG

Valice Raffi on tue 20 jan 04


I'd use PC-7 after roughing up the marble. If it's a large piece, I'd also
drill through both and have a bolted rod for added assurance.

Valice
tired of the fog in Sacramento

>Any suggestions for joining earthenware sculpture to marble bases? Would
>E-6000 be a good choice for this too? PG

Krista Peterson on wed 21 jan 04


I second the motion for PC7. I have glued some pretty heavey pieces together and hung them on the wall. Incredible stuff! You can get it in white too, PC11.

Krista Peterson

-----Original Message-----
From: Valice Raffi
Sent: Jan 20, 2004 8:21 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: joining earthenware to marble

I'd use PC-7 after roughing up the marble. If it's a large piece, I'd also
drill through both and have a bolted rod for added assurance.

Valice
tired of the fog in Sacramento

>Any suggestions for joining earthenware sculpture to marble bases? Would
>E-6000 be a good choice for this too? PG

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.