In a message dated 1/21/04 11:57:41 AM, selsor@IMT.NET writes:


> Hi Susan,
> I get my best colors in Raku when doing a post firing reduction at minus
> 20 F. in Montana.
> What can I say, it doesn't often happen that I am doing raku then. But
> that is when the colors are best!
> Marcia Selsor
> not in Montana at the moment.
>
>

We got some not-so-great colors on Sunday but the kiln got away from us and I
think my piece, which was pulled just about last, was over-cooked some.