Mike Gordon on tue 20 jan 04


I've been using plaster wedging tables for 40yrs with no problems at
all. If you look in the kitchen cleaning section of the grocery store
you will find plastic scrubbers in the shape of a ball. They are soft
like a ball of string, thin strands of plastic woven together. flood
the surface with water and scrub clean! Very easy & cheap. Mike Gordon

Mildred Herot on wed 21 jan 04


I made myself a plaster wedging board over 40 years ago and it still works
fine. What I like to clean it with is a plastic trowel used in grouting
tile.....Mildred Herot-----
From: "Mike Gordon"
To:
Sent: Tuesday, January 20, 2004 10:28 PM
Subject: cleaning plaster wedging tables


> I've been using plaster wedging tables for 40yrs with no problems at
> all. If you look in the kitchen cleaning section of the grocery store
> you will find plastic scrubbers in the shape of a ball. They are soft
> like a ball of string, thin strands of plastic woven together. flood
> the surface with water and scrub clean! Very easy & cheap. Mike Gordon
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.