dale's iron saturate glaze ^6

updated mon 26 jan 04

 

John Rodgers on thu 22 jan 04


I saw a glaze called Dale's Iron Saturate glaze and was wondering if
anyone has the formula for it. I didn't find anything in the archives on
it. In fact, every time I did a search for iron satuarate I got nothing.

Does anyone have this glaze recipe. I don't know the original source.

Thanks,

John Rodgers
Chelsea, AL

John Rodgers on fri 23 jan 04


My thanks to all who have responded.to my request. I now have the glaze.
Will give it a try and report back to Clayart the results.

Regards,

John Rodgers

Chelsea, AL

John Rodgers wrote:

> I saw a glaze called Dale's Iron Saturate glaze and was wondering if
> anyone has the formula for it. I didn't find anything in the archives on
> it. In fact, every time I did a search for iron satuarate I got nothing.
>
> Does anyone have this glaze recipe. I don't know the original source.
>
> Thanks,
>
> John Rodgers
> Chelsea, AL
>
> ______________________________________________________________________________
>
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>

Ababi on sat 24 jan 04


In the site are all the recipes

Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm



-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Marianne
Lombardo
Sent: Friday, January 30, 2004 4:08 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: Dale's Iron Saturate glaze ^6

Photos of this glaze, and the recipe are found at Stephen Pilachowski's
site:

http://members.bellatlantic.net/~spilacho/

Marianne Lombardo
Omemee, Ontario, Canada


> I saw a glaze called Dale's Iron Saturate glaze and was wondering if
> anyone has the formula for it. I didn't find anything in the archives
on
> it. In fact, every time I did a search for iron satuarate I got
nothing.
>
> Does anyone have this glaze recipe. I don't know the original source.

________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Robert Seele on mon 26 jan 04


John,

Try looking here, under recipie.

> http://members.bellatlantic.net/~spilacho/index.htm


On Thursday, January 22, 2004, at 08:33 PM, John Rodgers wrote:

> I saw a glaze called Dale's Iron Saturate glaze and was wondering if
> anyone has the formula for it. I didn't find anything in the archives
> on
> it. In fact, every time I did a search for iron satuarate I got
> nothing.
>
> Does anyone have this glaze recipe. I don't know the original source.
>
> Thanks,
>
> John Rodgers
> Chelsea, AL
>
> _______________________________________________________________________
> _______
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
>
Bob Seele
Nicely outside of Chicago
Things should be made as simple as possible, but not any simpler :
Albert Einstein

Marianne Lombardo on fri 30 jan 04


Photos of this glaze, and the recipe are found at Stephen Pilachowski's
site:

http://members.bellatlantic.net/~spilacho/

Marianne Lombardo
Omemee, Ontario, Canada


> I saw a glaze called Dale's Iron Saturate glaze and was wondering if
> anyone has the formula for it. I didn't find anything in the archives on
> it. In fact, every time I did a search for iron satuarate I got nothing.
>
> Does anyone have this glaze recipe. I don't know the original source.