Reid Harvey on tue 3 feb 04
Friends and Colleagues,
Please check the following link to our update:
http://www.purifier.com.np/spgrog.php
This introduces a new type of household water purification system,
consisting of silver saturated grog, pre fired clay, within pvc pipe
parts. As with our candle purifiers we expect these particulate
purifiers to give virtually 100% removal of the fecal coliform
indicators, as well as being appropriate and low cost for the poor.
Regards,
Reid Harvey
Ceramic Designer
Pottery Water Purifier Project, Nepal
http://www.purifier.com.np
Tel. (977-1) 5521 889 or 9810 49142
| |
|