John Rodgers on fri 6 feb 04
I'm looking for the chemical analysis of Ferro Frit 3289 to be used in
Peacock Blue II glaze as posted by Sandy Miller back in May, 2003. I
think this glaze may have originated with Karen Gringus but I got my
recipe from the post by Sandy.
I need the Frit analysis to put into JH & RR 's "Glazemaster" software.
I looked at a couple of websites with frits, but didn't find this one.
Does anyone have this analysis???
Thanks,
John Rodgers
Chelsea, AL
Cindy Gatto on fri 6 feb 04
Hi John,
I have the Standard Clay co. catalog which has the analysis for frit #3289 It
is ;
Na2O-5.5
BaO -27.4
Al2O3- 5.4
B2O3- 12.4
SiO2- 49.3 Hope this helps.
Cindy & Mark
The Mudpit
228 Manhattan Ave
Brooklyn, NY 11206
718-218-9424
mudpitnyc@aol.com
www.mudpitnyc.com
Frank Gaydos on sat 7 feb 04
24.Ferro Frit 3289
M.P./¡F 1500
Silica/Alumina ratio: 15.5:1
Equivalent Molecular Weight: 374.127
Molecular Formula of Ferro Frit 3289:
Na2O 0.332 Al2O3 0.198 SiO2 3.070
BaO 0.668 B2O3 0.668
Percentage Analysis
49.30 % SiO2
5.40 % Al2O3
5.50 % Na2O
27.40 % BaO
12.40 % B2O3
______________
100 % TOTAL
Comments: 8.2 x 10-6 coefficient of thermal expansion (50-450¡ C)
http://mysite.verizon.net/vze778gn/frits.html
----- Original Message -----
From: "John Rodgers"
To:
Sent: Friday, February 06, 2004 9:58 AM
Subject: Frit 3289 Analysis
> I'm looking for the chemical analysis of Ferro Frit 3289 to be used in
> Peacock Blue II glaze as posted by Sandy Miller back in May, 2003. I
> think this glaze may have originated with Karen Gringus but I got my
> recipe from the post by Sandy.
>
> I need the Frit analysis to put into JH & RR 's "Glazemaster" software.
>
> I looked at a couple of websites with frits, but didn't find this one.
>
> Does anyone have this analysis???
>
> Thanks,
>
> John Rodgers
> Chelsea, AL
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
| |
|