search  current discussion  categories  materials - paper clay 

paperclay and sawdust firing

updated sat 14 feb 04

 

Patricia Gilmartin on fri 13 feb 04


Has anyone had any experience with firing paper clay items in a sawdust
firing? Seems like it ought to work because the paper burns out and
leaves the clay more "open." Can you burnish paper clay successfully? It
is necessary to bisque fire before putting the paper clay in the
sawdust?
Pat Gilmartin