search  current discussion  categories  glazes - misc 

resources on glaze formulation

updated sun 22 feb 04

 

Ivor and Olive Lewis on thu 19 feb 04


Dear Brian,
No better place to start than "Mastering Cone Six Glazes" By Ron Roy
and John Hesselberth which gives you simple reasons why you have to do
what is needed to be done to bypass the problems. Web contact via
http://www.masteringglazes.com
Then, to see the breadth of what can be achieved get Greg Daly's book
details of which I gave yesterday. It is a real "How to do'
experience.
Best regards,
Ivor Lewis. Redhill, South Australia

stephen h on thu 19 feb 04


try clay and galzes for the potter the third edition by robin hopper,,,, ian currie's stoneware glazes,,,,, the ceramic glaze handbook second edition.

stephen h



---------------------------------
Do you Yahoo!?
Yahoo! Mail SpamGuard - Read only the mail you want.

daniel on thu 19 feb 04


Hi Brian,

You are gonna get a lot of help on this one from this list :)

I'm not really qualified but I'm chasing glaze theory a lot lately and
prepping to do a bunch of different tests and so on. Books that I have and
am reading on this are Harry Frazer's Glazes for the Craft Potter (only just
got it and love it), Robin Hopper's Ceramic Spectrum (in my view a great
book on the topic), Mark Burleson's The Ceramic Glaze Handbook. All of these
have technical bits in them but not as technical as it can get. They explain
about materials and the compositions and oxides and all that. Burleson's is
nice because it has a bunch of photos of the materials themselves. As
someone who has yet to get a lot of materials to look at its really good to
see them. These books have a bunch on mixing, testing, applying glazes and
so on.

If you are looking for something about glazes of a specific type eg. cone
6, raku etc. there are some around. Others on the list will no doubt help
out with these. If you're into mixing up dirt and stuff there are books on
that too. Let us know more about what you're into and that will help a
little.

HTH
D

b_boz_99 writes:

> Hello,
>
> I am an hobby potter and am wanting to learn more about
> formulating my own glazes. Does anyone know of any books or other
> resources that I might use to teach myself the basics? Nothing to
> technical..
> Brian
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.

Lawrence Ewing on thu 19 feb 04


Hi Brian,

You might like to have a look at GlazeTeach.

http://www.Matrix2000.co.nz/GlazeTeach

Cheers,

Lawrence Ewing

21 Slant St
Careys Bay
Dunedin
New Zealand

EMAIL: lewing@clear.net.nz

URLS:
Matrix Glaze Software:
http://www.Matrix2000.co.nz
Glaze Chemistry Instruction:
http://www.Matrix2000.co.nz/GlazeTeach/Index.htm
New Zealand Society of Potters website:
http://www.nzPotters.com
----- Original Message -----
From: "b_boz_99"
To:
Sent: Thursday, February 19, 2004 4:08 PM
Subject: Resources on Glaze Formulation


> Hello,
>
> I am an hobby potter and am wanting to learn more about
> formulating my own glazes. Does anyone know of any books or other
> resources that I might use to teach myself the basics? Nothing to
> technical..
> Brian
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>

b_boz_99 on thu 19 feb 04


Hello,

I am an hobby potter and am wanting to learn more about
formulating my own glazes. Does anyone know of any books or other
resources that I might use to teach myself the basics? Nothing to
technical..
Brian

May Luk on sat 21 feb 04


Did anybody mention David Hewitt's site.

http://www.dhpot.demon.co.uk/

I found it very useful. If you want to read some more after Glazes Cone 6
[Micheal Bailey]

So much info, so little time

Regards
May
London, UK