search  current discussion  categories  glazes - misc 

glaze tests/mary

updated sat 21 feb 04

 

Alisa Clausen on fri 20 feb 04


Hi Mary,
I will do the tests in the small kiln and fire pots in the larger, as a
rule. But rules are broken.
The baby is small, but it is not tiny. It is 120 liters. I am firing a
bisque now. I control my
cool down, so it will be interesting to see if I do get the same glaze
results from both kilns.
Will post the photos as I get results.

regards from Alisa in Denmark