I agree with you Michael, especially when you tell us that this is at =
Cone 10 and you have two of the most prominent fluxing oxides , MgO and =
CaO, in your mixture.=20
I think the process is called "Liquid Phase Sintering"

Best Regards,
Ivor Lewis. Redhill, South Australia