Imbolchottie@AOL.COM on mon 23 feb 04


When I was mixing up a batch of glaze this week I found that our studio had
run out of EPK which is needed for the 20 x 5 glaze. I did, however, find that
I had enough Calcined Clay on hand.

Question is -- Is this a good substitute, or a bad substitute?

Jonathan