Chirs Greenman on thu 26 feb 04
Wellllllllllll,
Thank you very much for those that responded with input on this kiln. I have
experienced some cracking with our kiln. Long horizontal cracks--not good.
My thinking now is that I will go ahead and bisque next week anyway and
repair the kiln with kiln patch and coat with ITC. I am going strategically
(I hope wire the kiln together before firing. I will let you all know what
happens.
Chris
In Montgomery where it is very damp
| |
|