In the Grace's "B" Base,
the original recipe calls for
Adding
5 Bentonite
5 Tin ox.

I admitted these additions in my tests, and colored the base as =
described in the post.

In the glaze test Randi's Red and revision, I wrote that I subbed Kona =
F-4 with Ball Clay.
That was a written error. The sub. was for Forshammer feldspar.

Note: All recipes are in the archives, both new and old that are shown =
on the Yahoo page.
My website is a disaster and until further notice, is down. Was not a =
good trade afterall.