Alisa Clausen on thu 4 mar 04


I liked some of the glazes I just tested, both the B Base and the =
Raspberry Base, with the Chrome a la carte (fumed). Also the Pinnell =
Strontium Mat and the Metallic Black I use for decorative spots on =
decorative pots. These pots are a series called Cracked open, to be egg =
like with mat outsides and glossier insides. Also some pots moving in =
the spring.