Nicol on thu 11 mar 04
If a design is made with pencil or carbon paper (transfer paper) on white
commercial bisque tile, will it burn out after applying underglazes and then
dipping the tile in clear glaze ??? --- or will it still be visible after a
^06 firing?? I am doing a couple of projects some local youth and would
like to allow them to put their rough designs on the bisque tile before they
are glazed with the hope that after glazing and firing the initial "sketch"
will be gone.
Michele Jurist on thu 11 mar 04
It will burn out.
Regards, Michele
----- Original Message -----
From: "Nicol"
To:
Sent: Thursday, March 11, 2004 5:07 PM
Subject: ^06 burn out
> If a design is made with pencil or carbon paper (transfer paper) on white
> commercial bisque tile, will it burn out after applying underglazes and
then
> dipping the tile in clear glaze ??? --- or will it still be visible after
a
> ^06 firing?? I am doing a couple of projects some local youth and would
> like to allow them to put their rough designs on the bisque tile before
they
> are glazed with the hope that after glazing and firing the initial
"sketch"
> will be gone.
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
Snail Scott on fri 12 mar 04
At 08:07 PM 3/11/04 -0500, you wrote:
>If a design is made with pencil or carbon paper (transfer paper) on white
>commercial bisque tile, will it burn out after applying underglazes and then
>dipping the tile in clear glaze ??? --- or will it still be visible after a
>^06 firing??
Pencil marks will burn out and so will pure carbon,
but...carbon paper often holds the carbon in place
with wax, which can resist glaze. Use homemade
carbon paper instead: make the drawing, then rub
the back with soft graphite pencil and retrace
the drawing in place on the tile. Note that very
heavy graphite lines can resist glaze, too, so keep
it light!
-Snail
| |
|