=?iso-8859-1?q?Iben=20Vedel?= on fri 12 mar 04


Sorry, got my head in the clouds, here is the recipe:

Turquise/Oxblood glaze.
Potash Feldspar 420
Whiting 210
Silica 210
Kaolin 100
Talc 50
Tin Oxide 75
Copper Carbonate 10

Fires to 1250C Oxidation or Reduction.