Marianne Lombardo on sun 21 mar 04
HANDCREAM (FOR OFTEN-WET HANDS)=20
200g Baby Powder (talcum powder)=20
200g Vaseline ( petroleum jelly)=20
50ml Glycerine=20
50ml Eucalyptus oil.=20
Mix all together, being careful not to breathe in 'dust'=20
from Toni Martens=20
John Rodgers on mon 22 mar 04
Marianne, thanks for posting this. I couldn't for the life of me
remember who I got the recipe from. It was Toni!!!
And I do like the handcream. Works for me.
John Rodgers
Chelsea, AL where it looks like it is snowwing, what with all the pear
blossoms falling from the trees around the house.
Marianne Lombardo wrote:
>HANDCREAM (FOR OFTEN-WET HANDS)
>
>200g Baby Powder (talcum powder)
>200g Vaseline ( petroleum jelly)
>50ml Glycerine
>50ml Eucalyptus oil.
>Mix all together, being careful not to breathe in 'dust'
>from Toni Martens
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>
>
>
| |
|